Why After Spraying Has Poor Leveling Performance, With ObviousOrange Peel?

Views: 0     Author: Site Editor     Publish Time: 2024-01-17      Origin: Site

Why After Spraying Has Poor Leveling Performance, With Obvious Orange Peel? 1. Coating is toothick or too thin Solution: Control the coating thickness by adjusting the coating equipment2. Baking temperature is too low Solution: Adjust the baking temperature to the correct value